carbon steel welding rods & mild steel welding rods e6013
Description:
Welding Electrodes AWS E6013 is a low carbon steel electrode with high titanium-potassium type coating and suitable for both AC and DC. The electrode is able to provide excellent welding technological performance because the arc is extra stable and spatter loss is negligible, the slag has good fluid and solidified slag is very easy to remove, the manipulate is free and restrike is easy. It can give smooth and beautiful ripples.
Applications:
Mild steel fabrications, Steel windows and iron grills and fences, container steel, welding of ungalvanized pipes, steel structures for houses, steel chairs and tables, steel ladders and other light gauge mild steels and others.
Characteristics:
No smoke and odorless
Few and fine spatterings
Steady and smooth arc
Self removing slag reduces cleaning time
Strong and high quality weld metal properties
Typical Chemical Composition of Weld Metal (%):
C | Mn | Si | P | S |
0.09 | 0.38 | 0.26 | 0.015 | 0.012 |
Typical Mechanical Properties of Weld Metal:
Yield Point N/mm2 (Kgf/mm2) | Tensile Strength N/mm2 (Ksi) | Elongation (%) | Impact Value Deg C, J (Deg F, Ft-lbs) |
420 (61) | 490 (71) | 30 | 0, 90 (32, 66) |
Size and Recommended CurrentRange (AC or DC +/-):
Diameter (mm) | 1.6 | 2.0 | 2.5 | 3.2 | 4.0 | 5.0 | |
Length (mm) | 275 | 275 | 350 | 350 | 400 | 400 | |
Ampere | Flat | 20-45 | 30-65 | 60-95 | 90-130 | 120-170 | 150-220 |
V&OH | 20-45 | 30-65 | 60-62 | 90-130 | 125-160 | 125-190 |
Welding position:
Notes on Usage
(1) Pay attention not to exceed the range of proper currents. Welding with excessive current not only lowers X-ray soundness, but also causes increase of spatter, under-cut and insufficient slag covering.
(2) Dry the electrodes at 70-100 degrees C for 30-60 minutes before use. Excessive moisture absorption lowers usability and may result in some porosities.
(3) Excessive drying before use causes less in penetration and overheating of the electrode.
Business type:manufacturer(more than 30years)
Certificate:ISO CE AWS SONCAP SGS BV
.
factory manufacturer !carbon steel welding rods & mild steel welding rods e6013